ibhena_yephepha

iimveliso

I-Polyester Resin engagcwaliyo ye-Frp

inkcazo emfutshane:

I-resin ye-189 yi-resin ye-polyester engagcwaliyo ene-benzene tincture, i-cis tincture kunye ne-glycol eqhelekileyo njengezinto eziphambili ezisetyenzisiweyo. Inyibilikisiwe kwi-styrene cross-linking monomer kwaye ine-viscosity ephakathi kunye ne-medium reactivity.


Iinkcukacha zeMveliso

Iithegi zeMveliso


IMPAHLA

•I-resin eli-189 ihlangabezana neemfuno zesatifikethi se-China Classification Society (CCS).
•Ineengenelo zokuba namandla alungileyo, ukuqina kunye nokuphiliswa ngokukhawuleza.

ISICELO

•Ifanelekile ukwenza izinto zobugcisa ngezandla ukuze kwenziwe iimveliso ezahlukeneyo ezixhathisa amanzi ezifana neenqanawa zeplastiki eziqinisiweyo zeglasi, iinxalenye zeemoto, iinqaba zokupholisa, izinki, njl.njl.

ISALATHISO SOMGAQO

 INTO  Uluhlu  Iyunithi Indlela yoVavanyo

Inkangeleko

Umbala otyheli okhanyayo
Ubumuncu 19-25 mgKOH/g GB/T 2895-2008

Ukuxinana, ii-cps ezingama-25℃

0. 3-0. 6 Pa.s GB/T 2895-2008

Ixesha lejeli, ubuncinci 25℃

12-30 umzuzu GB/T 2895-2008

Umxholo oqinileyo, %

59-66 % GB/T 2895-2008

Uzinzo lobushushu,

80℃

≥24 h GB/T 2895-2008

Iingcebiso: Ukufumanisa Ixesha Lokuhlanjwa KweeGelation: 25°C amanzi okuhlamba, 50g ye-resin ene-0.9g T-8m (NewSolar, L % CO) kunye ne-0.9g M-50 (Akzo-Nobel)

IMEMO: Ukuba uneemfuno ezikhethekileyo zeempawu zokuphilisa, nceda unxibelelane neziko lethu lobugcisa

IPROPATHI YOMKHANIKI YE-CASTING

INTO  Uluhlu

 

Iyunithi

 

Indlela yoVavanyo

Ubulukhuni beBarcol

42

GB/T 3854-2005

Ukuphambuka kobushushutumbuso

60

°C

GB/T 1634-2004

Ukwandiswa ngexesha lokuphumla

2.2

%

GB/T 2567-2008

Tensile strength

60

I-MPa

GB/T 2567-2008

Imodulus yokutsalwa

3800

I-MPa

GB/T 2567-2008

Amandla okuGuquka

110

I-MPa

GB/T 2567-2008

Imodulus eguquguqukayo

3800

I-MPa

GB/T 2567-2008

IMEMO: Idatha edwelisiweyo yipropati eqhelekileyo, ayifanele ithathwe njengenkcazelo yemveliso.

IMPAHLA YE-FRP

INTO Uluhlu

Iyunithi

Indlela yoVavanyo

Ubulukhuni beBarcol

64

GB/T 3584-2005

Tensile strength

300

I-MPa

GB/T 1449-2005

Imodulus yokutsalwa

16500

I-MPa

GB/T 1449-2005

Amandla okuGuquka

320

I-MPa

GB/T 1447-2005

Imodulus eguquguqukayo

15500

I-MPa

GB/T 1447-2005

IMIYALELO

• I-resin eyi-189 ine-wax, ayinazo izinto ezikhawulezisayo kunye nezongezo ze-thixotropic.
• Kucetyiswa ukuba ukhethe ii-resin ze-/IO Peng Liu? Ortho-phthalic 9365 series ezineemfuno zokusebenza eziphezulu.

 

UKUPAKISHA NOKUGCINA

• Imveliso mayipakishwe kwisikhongozeli esicocekileyo, esomileyo, esikhuselekileyo nesivalekileyo, ubunzima obupheleleyo obuyi-220 Kg.
• Ixesha lokugcinwa: Iinyanga ezi-6 ngaphantsi kwama-25℃, zigcinwe kwindawo epholileyo necocekileyo
indawo enomoya.
• Nasiphi na imfuneko ekhethekileyo yokupakisha, nceda unxibelelane neqela lethu lenkxaso

PHAWULA

• Lonke ulwazi olukule khathalogu lusekelwe kwiimvavanyo eziqhelekileyo ze-GB/T8237-2005, kuphela ngenjongo yokubhekisela; mhlawumbi zahluke kwidatha yovavanyo lokwenyani.
• Kwinkqubo yokuvelisa iimveliso ze-resin, kuba ukusebenza kweemveliso zomsebenzisi kuchatshazelwa zizinto ezininzi, kuyimfuneko ukuba abasebenzisi bazivavanye ngaphambi kokuba bakhethe kwaye basebenzise iimveliso ze-resin.
• Iiresini zepolyester ezingagcwaliyo azizinzanga kwaye kufuneka zigcinwe ngaphantsi kwama-25°C emthunzini opholileyo, zihanjiswe kwikhareji okanye ebusuku, ziphephe ukukhanya kwelanga.
•Nayiphi na imeko engafanelekanga yokugcina nokuhambisa impahla iya kubangela ukuba ixesha layo lokuphelelwa lixabiso lifutshane.


  • Ngaphambili:
  • Okulandelayo:

  • Uphando lwePricelist

    Ukuba unemibuzo malunga neemveliso zethu okanye uluhlu lwamaxabiso, nceda usishiyele i-imeyile yakho kwaye siya kuqhagamshelana nathi kwiiyure ezingama-24.

    COFA UKUZE UFAKE UMBUZO