• I-MFE 770 vinyl ester resin yi-epoxy novolac-based resin eyenzelwe ukubonelela ngeempawu ezikhethekileyo ze-thermal kunye neekhemikhali zokumelana namaqondo aphezulu. Inika ukuchasana okuphezulu kwi-solvents kunye neekhemikhali, ukugcinwa kakuhle kwamandla kunye nokuqina kumaqondo obushushu aphakamileyo, kunye nokuchasana okugqwesileyo kwiindawo ezine-acidic oxidizing.
• Izixhobo ze-FRP eziveliswe kusetyenziswa i-MFE 770 zigcina amandla kunye nokuqina kumaqondo obushushu aphakamileyo.
•I-MFE 770 sisizukulwana sesibini se-MFE W1 (W2-1) esele isetyenziswe ngempumelelo kwimisebenzi yoshishino enzima kwiminyaka emininzi kwaye ibonelela ngenye indlela yoqoqosho kwiialloys zangaphandle ngokuvumela ukusetyenziswa kwexabiso eliphantsi le-FRP kwizinto eziqhelekileyo.
•Izilungele izicelo ezifana neenkqubo ze-FGD, izibonelelo zokucocwa kwenkunkuma kwimizi-mveliso, ukucholwa kwesinyithi kunye neenkqubo zokutsalwa kwezinyibilikisi ezisetyenziswa emigodini.
• Inkqubo yokwenziwa kwe-FRP kuquka ukubunjwa koqhagamshelwano (ukubekwa kwesandla), ukutshiza, i-pultrusion, i-infusion (RTM), njl.
•Ukwenziwa kotyatyazo olunzima lokunqanda ukubola okufana neflake yeglasi.
•Ukuba ufuna ukumelana nobushushu obuphezulu, nceda ucinge nge-MFE 780(i-HDT 160-166 °C)
I-MFE 780HT-300 (iphosa i-HDT 175 °C) okanye i-MFE 780HT-750 (iphosa i-HDT 200-210 °C).
IiPropathi eziQhelekileyo zeResin yolwelo
Ipropati(1) | Ixabiso |
Viscosity, cps 25℃ | 230-370 |
Isiqulatho seStyrene | 34-40% |
Beka ubomi kwishelufa(2) Kumnyama, 25℃ | Iinyanga ezi-6 |
(1)Amaxabiso aqhelekileyo, akanakwakhiwa njengengcaciso
(2)Igubu elingavulwanga elingenazo zongezelelo, abakhuthazi, ii-accelerators, njl. Ubomi beshelufu buchaziwe ukusuka kumhla wokwenziwa.
Iinkcazelo Ngeempawu eziQhelekileyo (1) Intlaka eCacileyo yokuSasa (3)
Ipropati | Ixabiso | Indlela yoVavanyo |
Amandla Okuqina/MPa | 75-90 | |
I-Tensile Modulus/GPa | 3.4-3.8 | I-ASTM D-638 |
Ubude ngexesha lekhefu / % | 3.0-4.0 | |
Amandla e-Flexural/ MPa | 130-145 | |
I-ASTM D-790 | ||
Flexural Modulus / GPa | 3.6-4.1 | |
HDT(4) / °C | 145-150 | I-ASTM D-648 Indlela A |
Ukuqina kweBarcol | 40-46 | I-ASTM D2583 |
(3)Ishedyuli yonyango: iiyure ezingama-24 kwiqondo lobushushu begumbi; Iiyure ezi-2 kwi-120₰C
(4) Uxinzelelo olukhulu: 1.8 MPa
Ukuqwalaselwa koKhuseleko nokuPhatha
Le resin iqulethe izithako ezinokuba yingozi xa ingaphathwanga kakuhle. Ukudibana nolusu kunye namehlo kufuneka kuphetshwe kwaye izixhobo eziyimfuneko zokukhusela kunye nempahla kufuneka inxibe. Inkcazo yi-2012 edition kwaye inokutshintsha ngophuculo lobuchwepheshe.
I-Sino Polymer Co., Ltd. igcina i-Material Safety Data Sheets kuzo zonke iimveliso zayo. Amaxwebhu eNkcukacha yoKhuseleko lweMathiriyeli aqulethe ulwazi lwezempilo kunye nokhuseleko kuphuhliso lwakho lweenkqubo ezifanelekileyo zokuphatha imveliso ukukhusela abasebenzi bakho kunye nabathengi. IiNkcukacha zethu zoKhuseleko lweMathiriyeli kufuneka zifundwe kwaye ziqondwe ngabo bonke abasebenzi bakho abaphantsi kolawulo kunye nabasebenzi ngaphambi kokusebenzisa iimveliso zethu kumaziko akho.
Ugcino oluCetyisiweyo:
Amagubu - Gcina kumaqondo obushushu angaphantsi kwe 25℃. Ubomi bogcino buyancipha ngokunyuka kobushushu bokugcina. Kuphephe ukuchanabeka kwimithombo yobushushu efana nelanga elithe ngqo okanye imibhobho yomphunga. Ukuze ugweme ukungcoliswa kwemveliso ngamanzi, musa ukugcina ngaphandle.
Keep sealed to prevent moisture pick-up and monomer loss. Rotate stock. For more information, please contact us at sale1@frp-cqdj.com
Umqulu:200kg igubu lentsimbi nganye okanye 1000kg nganye IBC