ngenxa yoncedo olugqwesileyo, iintlobo ngeentlobo zeemveliso ezikumgangatho ophezulu kunye nezisombululo, iindleko ezindlongondlongo kunye nonikezelo olusebenzayo, siyakuvuyela ukuthandwa okubalaseleyo phakathi kwabathengi bethu. Silishishini elikhutheleyo elinentengiso ebanzi ye-E-Glass Fiber Chopped Strand Mat EMC600g i-Emulsion/Powder, Ngoku siye savelisa igama elinoxanduva phakathi kwabathengi abaninzi. Umgangatho kunye nomthengi kuqala zidla ngokusukela rhoqo. Sizama kangangoko ukunceda ukwenza izisombululo ezingcono kakhulu. Jonga phambili kwintsebenziswano yexesha elide kunye neenzuzo ezifanayo!
ngenxa yoncedo olugqwesileyo, iintlobo ngeentlobo zeemveliso ezikumgangatho ophezulu kunye nezisombululo, iindleko ezindlongondlongo kunye nonikezelo olusebenzayo, siyakuvuyela ukuthandwa okubalaseleyo phakathi kwabathengi bethu. Sishishini elinamandla kunye nemarike ebanziChina Fiberglass Mat kunye wanqunqa Strand Mat, Ukwenza iimpahla ezithe kratya zokuyila, ukugcina iimpahla ezikumgangatho ophezulu kunye nokuhlaziya kungekuphela nje ukuthengisa kwethu kodwa nathi ukuze sisigcine siphambi kwehlabathi, kunye nelokugqibela kodwa elibaluleke kakhulu: ukwenza wonke umxhasi aneliseke ngayo yonke into esiyibonelelayo kwaye sikhule. bomelele kunye. Ukuze ube ngoyena mntu uphumeleleyo, qala apha!
1. Ukubekwa kwesandla: Ukubekwa kwezandla yeyona ndlela iphambili yokuvelisa i-FRP. Iimethi ze-Fiberglass ezinqunqiweyo, iimethi eziqhubekayo, kunye neemethi ezithungelweyo zingasetyenziselwa ukubeka izandla. Ukusetyenziswa kwe-ai-stitch-bonding matinokunciphisa inani leeleya kunye nokuphucula ukusebenza kakuhle kwemisebenzi yokubeka izandla. Nangona kunjalo, ngenxa yokuba i-stitch-bonded mat inemicu ye-fiber stitchbonding, amaqamza akulula ukuwagxotha, iimveliso zefiberglass zinamaqamza amile njengenaliti, kwaye umphezulu uvakala urhabaxa kwaye awugudi. Ukongeza, i-mat edibeneyo yilaphu elinzima, kwaye i-mold coverage ifutshane kune-mat esikiweyo kunye ne-mat eqhubekayo. Xa usenza iimveliso ezinemilo enzima, kulula ukwenza i-voids kwi-bend. Inkqubo yokubeka isandla ifuna ukuba i-mat ibe neempawu zesantya sokungena ngokukhawuleza kwe-resin, ukupheliswa okulula kwamaqamza omoya, kunye nokugubungela kakuhle ukungunda.
2. I-pultrusion: Inkqubo ye-pultrusion yenye yezona zinto zisetyenziswayo ngokuqhubekayo ukuvakalelwa kunyeiimethi ezithungelweyo. Ngokubanzi, isetyenziswa ngokudityaniswa nokujikeleza okungajikwanga. Ukusebenzisaimathi eqhubekayokunye ne-mat ethungelweyo njengemveliso ye-pultruded inokuphucula kakhulu ihupula kunye namandla anqamlezayo emveliso kwaye ithintele imveliso ekuqhekekeni. Inkqubo ye-pultrusion idinga ukuba i-mat ibe nokusabalalisa ifayibha efanayo, amandla aphezulu aphezulu, izinga lokungena ngokukhawuleza kwe-resin, ukuguquguquka okulungileyo kunye nokuzaliswa kwe-mold, kunye ne-mat kufuneka ibe nobude obuqhubekayo.
I-3.RTM: Ukubunjwa kwe-resin transfer (RTM) yinkqubo yokubumba evaliweyo. Iqulethwe ngama-half-moulds, i-mold female kunye ne-mold yendoda, ipompo yoxinzelelo kunye ne-injection gun, ngaphandle kokushicilela. Inkqubo ye-RTM ngokuqhelekileyo isebenzisa i-stitch-boled mats eqhubekayo kunokuba i-strand mats enqunqiweyo. I-mat sheet iyafuneka ukuba ibe neempawu zokuba i-mat sheet kufuneka ihluthiswe ngokulula nge-resin, i-air permeability elungileyo, ukuxhathisa okulungileyo kwe-resin scour kunye nokugqithiswa kakuhle.
4. Inkqubo yokuvala:iimethi zomcu ezinqunqiweyokunye neemethi eziqhubekayo zisetyenziselwa ukujija kunye nokwenza i-resin-rich rich layers ezisetyenziselwa iimveliso, kubandakanywa iileya zangaphakathi ze-lining kunye neeleya zangaphandle zangaphandle. Iimfuno ze-glass fiber mat kwinkqubo yokujija ngokusisiseko ziyafana nezo zikwindlela yokubeka isandla.
I-5.Centrifugal casting molding: i-strand mat eqoshiwe idla ngokusetyenziswa njengezinto eziluhlaza. I-strand mat enqunqiweyo ibekwe ngaphambili kwi-mold, kwaye emva koko i-resin yongezwa kwi-mold ejikelezayo evulekileyo, kwaye amaqamza omoya akhutshwa yi-centrifugation ukwenza imveliso ixinene. Iphepha le-mat liyafuneka ukuba libe neempawu zokungena lula kunye nokungena kakuhle komoya.
Iimethi zethu ze-fiberglass ziziindidi ezininzi: iimethi zomgangatho wefiberglass,iimethi ze-fiberglass ezinqunqiweyo, kunye neemethi ze-fiberglass eziqhubekayo. I-strand mat eqoshiwe ihlulwe ibe yi-emulsion kunyeiimethi zomgubo weglasi.
I-E-Glass inqunyulwe i-Strand Mat Emulsion | |||||
Isalathiso soMgangatho-1040 | |||||
225G | 300G | 450G | |||
Into yovavanyo | Ikhrayitheriya Ngokwe | Iyunithi | Umgangatho | Umgangatho | Umgangatho |
UHLOBO lweglasi | G/T 17470-2007 | % | R2O<0.8% | R2O<0.8% | R2O<0.8% |
I-ARENTE YOKUXHUMANISA | G/T 17470-2007 | % | SILANE | SILANE | SILANE |
Ubunzima beNdawo | GB/T 9914.3 | g/m2 | 225±45 | 300±60 | 450±90 |
Loyi Umxholo | GB/T 9914.2 | % | 1.5-12 | 1.5-8.5 | 1.5-8.5 |
Ukuqina koxinzelelo lweCD | GB/T 6006.2 | N | ≥40 | ≥40 | ≥40 |
Tension Amandla MD | GB/T 6006.2 | N | ≥40 | ≥40 | ≥40 |
Umxholo wamanzi | GB/T 9914.1 | % | ≤0.5 | ≤0.5 | ≤0.5 |
Inqanaba lokuBonelela | G/T 17470 | s | <250 | <250 | <250 |
Ububanzi | G/T 17470 | mm | ±5 | ±5 | ±5 |
Ukugoba amandla | G/T 17470 | MPa | Umgangatho ≧123 | Umgangatho ≧123 | Umgangatho ≧123 |
Imanzi ≧103 | Imanzi ≧103 | Imanzi ≧103 | |||
Imeko yoVavanyo | |||||
Ubushushu obugciniwe(℃) | 10 | Ukufuma kwe-Ambient(%) |
Sineentlobo ezininzi ze-fiberglass roving:iphaneli yokujikeleza,fafaza ujikeleza,I-SMC ijikeleza,ukuzulazula ngokuthe ngqo,c iglasi ukuzulazula, kunye ne-fiberglass roving for chopping.Ngenxa yoncedo olugqwesileyo, iintlobo ngeentlobo zeemveliso ezikumgangatho ophezulu kunye nezisombululo, iindleko ezindlongondlongo, kunye nonikezelo olusebenzayo, siyakuvuyela ukuthandwa okumangalisayo phakathi kwabathengi bethu. Silishishini elinamandla elinorhwebo olubanzi lokuHlolwa koMgangatho we-E-Glass Fiber Chopped Strand Mat EMC600g Emulsion/Powder Chopped Strand Mat, Ngoku siye savelisa igama elinoxanduva phakathi kwabathengi abaninzi. Umgangatho kunye nomthengi kuqala kuqhelekile ukuba sisukele rhoqo. Sizama kangangoko ukunceda ukwenza izisombululo ezingcono kakhulu.
Jonga phambili kwintsebenziswano yexesha elide kunye neenzuzo ezifanayo!
Ukuhlolwa koMgangatho wePaneli yeLuphahla yaseTshayina kunye ne-FRP yaMashidi oKufulela, Ukudala iimpahla ezithe kratya zokuyila, ukugcina iimpahla ezikumgangatho ophezulu kunye nokuhlaziya kungekuphela nje ukuthengisa kwethu kodwa ngokwethu ukusigcina siphambi kwehlabathi, kunye nelokugqibela kodwa elibaluleke kakhulu: ukwenza wonke umxhasi aneliseke ngayo yonke into esiyibonelelayo kwaye sikhule somelele kunye. Ukuba ngoyena mntu uphumeleleyo kuqala apha!
Ngemibuzo malunga neemveliso zethu okanye uluhlu lwamaxabiso, nceda ushiye i-imeyile yakho kuthi kwaye siya kuqhagamshelana kwiiyure ezingama-24.